    Solder paste on the board. Slightly overexposed I think but perhaps room to tweak the raw? You can clearly see the solder particles even in the type 5 paste

    Macro photo of board with solder paste on it. The back of the image is somewhat blurred.
    💬 1🔄 0⭐ 0

Replies

  • Nov 11, 2026, 7:12 PM

    Post reflow, definitely visible graping on some of the solder joints but I think it's probably going to work? I'll definitely add more flux all over the place when I reflow it to the carrier board and hopefully that will clean it up and give better results.

    This was my first time using T5 paste. I may have to look at N2 purging or something, or a higher activity flux?

    Nothing I see is giving me immediate "it won't work" red flags at least, I don't think there's any obvious shorts.

    Macro photo of WLCSPs on PCB showing shiny silicon
    A different angle of the board showing some incompletely coalesced solder joints
    💬 1🔄 0⭐ 0
  • Nov 11, 2026, 7:19 PM

    Low angle macro shots looking at WLCSP balls. For scale the STM32L431 is 0.35mm pitch, the FPGA is 0.4, most others are 0.4 or 0.5.

    The oscillator doesn't look great in terms of the solder actually coalescing. I might actually want to just add some flux and cook it before I put it on a carrier just to be sure.

    Angled view of STM32 balls looking mostly OK
    Angled view of FPGA balls lookign decent
    90 degree rotated view of same area
    Another rotated view
    💬 1🔄 0⭐ 0
  • Nov 11, 2026, 7:20 PM

    Not thrilled with the oscillator (the long skinny 4 ball BGA at left) either.

    Type 5 paste is definitely harder to work with than T4.

    Side view of the oscillator showing BGA balls sitting in incompletely coalesced solder
    💬 0🔄 0⭐ 0